Evaluation of degree of conversion, microtensile bond strength and mechanical properties of three etch-and-rinse dental adhesives

Abstract This study evaluated microtensile bond strength (µTBS), degree of conversion, modulus of elasticity and ultramicrohardness of three etch-and-rinse adhesives systems. The materials evaluated were: Ambar (FGM), Optibond (Kerr) and Magic Bond (Vigodent). The degree of conversion was analyzed by FTIR/ATR. To evaluate bond strength (μTBS) in dentin, 15 teeth (n = 5) were restored and sliced to obtain the specimens (0.8mm2). The dynamic ultra microhardness tester was used to evaluate the hardness and modulus of elasticity. The Magic Bond adhesive system showed lower µTBS than Ambar and O...