Mostrando 13-24 de 80 artigos, teses e dissertações.
-
13. Influência da adição de Sn na resistência à corrosão e na capacidade de recarga da liga Pb-1,5%Sn para grade positiva de baterias chumbo-ácido
RESUMO O presente trabalho teve como objetivo avaliar o processo de corrosão do Pb e da liga Pb-1,5%Sn quando submetidos à condição de ciclagem em meio de ácido sulfúrico, visando compreender a influência da adição de Sn na resistência à corrosão e na capacidade de recarga para grades positivas de baterias do Pb-ácido. As amostras de estudo fora
Matéria (Rio J.). Publicado em: 20/05/2019
-
14. Effect of sulfate on the pitting potential of austenitic stainless steels 18Cr8Ni and 17Cr6Mn5Ni in chloride media
Abstract Pitting corrosion resistance of two austenitic stainless steels, 18Cr8Ni (Type 304L or UNS S30403 stainless steel) and 17Cr6Mn5Ni, was evaluated in three electrolytic solutions containing a fixed concentration of 0.6M sodium chloride and different additions of sodium sulfate, 0.06M, 0.15M or 0.6M. Cyclic potentiodynamic polarization tests were perfo
REM, Int. Eng. J.. Publicado em: 2019-03
-
15. On the Global and Localised Corrosion Behaviour of the AA2524-T3 Aluminium Alloy Used as Aircraft Fuselage Skin
The aim of this work was to study the corrosion process of new aluminium alloy AA2524-T3 (Solution Heat Treated and Cold Worked), which is a promising substitute of the base line AA2024-T3 for aircrafts fabrication, by global and localised techniques in sodium chloride medium (0.05 mol L-1 NaCl). The open circuit potential results revealed a stochastic evolu
Mat. Res.. Publicado em: 14/01/2019
-
16. Effect of Aging Heat Treatment H950 and H1000 on Mechanical and Pitting Corrosion Properties of UNS S46500 Stainless Steel
The effect of aging temperature on mechanical and pitting corrosion properties of UNS S46500 was investigated. Tensile and Hardness tests were carried out and the microstructure was analyzed by optical microscopy, scanning electron microscopy and X-ray diffraction; Thermo-Calc simulations helped in the phase identification. Pitting corrosion properties were
Mat. Res.. Publicado em: 08/11/2018
-
17. Enhancement of Pitting Corrosion Resistance of Austenitic Stainless Steel Through Deposition of Amorphous/Nanocrystalline Oxy-nitrided Phases by Active Screen Plasma Treatment
In this research, AISI 304 austenitic stainless steels were efficient treatment using active screen plasma oxy-nitriding technique. The modified layers were characterized by X-ray photoelectron spectroscopy, X-ray diffraction, scanning electron microscopy, transmission electron microscopes, and atomic force microscopy. In addition, the pitting corrosion resi
Mat. Res.. Publicado em: 29/10/2018
-
18. Evaluation of Corrosion Resistance of Commercial Aluminum Alloys in Ethanol Solutions
In the present research, we studied the corrosion resistance of commercial aluminum alloys exposed to ethanol produced in the northeastern region of Argentina and to commercial ethanol as reference medium. Electrochemical tests of potentiodynamic polarization and weight loss were performed by immersion at temperatures below the boiling point of ethanol (25 �
Mat. Res.. Publicado em: 22/10/2018
-
19. Caracterización del comportamiento frente a la corrosión en soldaduras de recargue de aceros inoxidables superdúplex
ABSTRACT Superduplex stainless steels have a dual structure constituted approximately by 50% of ferrite and 50 % of austenite. This fact produces a good combination of mechanical properties and corrosion resistance. Thanks to these features their use is growing, mainly in the industries of paper, chemical, gas and oil. Surfacing welding is used for the manuf
Matéria (Rio J.). Publicado em: 19/07/2018
-
20. Análisis de la corrosión de uniones por soldadura fuerte de compósitos matriz cobre
ABSTRACT This work presents an electrochemical corrosion study in synthetic seawater of the dissimilar joint of TiC/Cu composite by brazing technique. Composites were machined by liquid infiltration without external pressure. This composite were joined with copper using a filler material constituted by an alloy of silver - copper and titanium powder. The com
Matéria (Rio J.). Publicado em: 19/07/2018
-
21. Efecto de la composición sobre el comportamiento frente a la corrosión de aceros inoxidables austeníticos y martensíticos
ABSTRACT The aim of this work is to study the electrochemical behavior of a series of stainless steels in NaCl solution (10000 ppm Cl-) at room temperature. Considering the differences in structures (austenitic and martensitic) and the composition of alloys, a relationship between their electrochemical behavior and PREN (Pitting resistance equivalent number)
Matéria (Rio J.). Publicado em: 19/07/2018
-
22. Resistencia a la corrosión de aleaciones Al-Cu en biodiesel
ABSTRACT The aim of the present work was to evaluate the susceptibility to corrosion in biodiesel of Al-Cu alloys directionally solidified: Al-4.5wt.%Cu and Al-15wt.% Cu, in function of the type of structure (columnar, equiaxed or columnar-to-equiaxed transition - CET) and chemical composition. Working electrodes were prepared with different types of alloy s
Matéria (Rio J.). Publicado em: 19/07/2018
-
23. Fracture Behavior and Fatigue Performance of Inconel 625
Inconel 625 is a nickel-based highly-resistant superalloy widely used in aerospace components, in the nuclear industry, and especially in the maritime industry. Materials such as Inconel 625 have been widely used in oil exploration of Brazilian pre-salt layers due to their excellent resistance to corrosion under tension, pitting and crevice corrosion by chlo
Mat. Res.. Publicado em: 25/06/2018
-
24. Corrosion Behavior of Plasma Nitrided and Nitrocarburised Supermartensitic Stainless Steel
Supermartensitic stainles steels (SMSS's) are a new generation of martensitic steels that have been increasingly used in oil and gas applications due to their adequate corrosion resistance and mechanical properties. In the present study, SMSS specimens (UNS S41425) were solution heat treated and air cooled followed by plasma nitriding and nitrocarburising at
Mat. Res.. Publicado em: 12/03/2018