Poisoning and regeneration of Pt-Pd/WO3-ZrO2 short paraffin isomerization catalysts
AUTOR(ES)
Canavese, Sergio, Finelli, Zunilda, Busto, Mariana, Benitez, Viviana M., Vera, Carlos R., Yori, Juan C.
FONTE
Química Nova
DATA DE PUBLICAÇÃO
2010
RESUMO
WO3-ZrO2 catalysts promoted with Pt and Pd were tested as paraffin isomerization catalysts using n-hexane as model compound. Sulfur and amine poisoning and regeneration tests were used to assess the impact of the addition of Pt and Pd on the deactivation resistance and regenerability. Pt and PtPd catalysts were the most active for n-hexane isomerization. The low activity of the Pd catalyst was attributed to poor Pd metal properties when supported over WO3-ZrO2 and to a decrease of the number of BrQnsted acid sites. PtPd was the only catalyst capable of full regeneration after S poisoning. Amine poisoning completely supressed the isomerization activity and the original activity could only be restored by calcination and reduction.
Documentos Relacionados
- Modification of the performance of WO3-ZrO2 catalysts by metal addition in hydrocarbon reactions
- PREPARATION AND PROPERTIES OF PT-RH-PD
- Desenvolvimento e caracterização de catalisadores de níquel suportados em matrizes CeO2-ZrO2-Al2O3, CeO2-La2O3-Al2O3 e ZrO2-La2O3-Al2O3 avaliados para as reações de reforma do metano
- "ZrO2/g-Al2O3-supported platinum catalysts for the steam reforming of ethanol"
- Dispersão de nanopartículas de ZrO2 visando produção de nanocompósitos de ZrO2 em matriz de Al2O3